Tribobond™ 34 Cr0N

Wear resistant coating with a top oxide layer

Tribobond 34 CrON features standard CrN coating with a top layer of CrON. Presence of the oxide film on the surface adds additional functionalities to the coating. Among those are decreased affinity to non-metallic materials, like elastomeric seals and components, lower friction in certain lubricating conditions, anti-sticking and improved resistance to stick-slip phenomenon and certain corrosive environments.  
The main and oxide layers are produced in a single coating cycle, so there is no need for additional processing.

Technical Data

 

Material

Cr0N

Technology

PVD Arc

Thickness range

2 - 5μm

Nanohardness, HV 0.005

1800 - 2200

Friction vs. Steel

<0.55

Service Temperature

180 - 350°C

Process Temperature

700°C

Color

Black/Rainbow