Tribobond™ 46 DLC
DLC coating for high temperature industrial components and high volume automotive applications
Ionbond’s Tribobond™ 46 DLC, CrN + a-C:H:W, coating is based on the excellent load bearing and high temperature properties of Tribobond™ 30 (CrN), with an extra low friction running-in coating on top. This results in a coating system that combines excellent running-in properties, a high load carrying capacity and fatigue resistance with a good wear resistance and a low coefficient of friction.
Performance
Hard and wear resistance coatings like Tribobond™ 46 DLC offer high load bearing capabilities combined with excellent counterparts protection in order to extend the lifetime of the components.

Technical data |
|
---|---|
Material |
Cr + CrN + a-C:H:W |
Coating thickness |
1 - 8 μm |
Service Temp. |
350 °C |
Deposition Temp. |
200 - 250 °C |
Hardness HV 0.05 |
1000 – 1800 (for the a-C:H:W top layer) |
Abrasive wear resistance |
2 – 7 * 10-15 m³/Nm |
Deposition method |
PVD UBM |
Friction vs. steel, dry |
0.1 |
Color |
grey |