Tribobond™ 46 DLC

DLC coating for high temperature industrial components and high volume automotive applications

Ionbond’s Tribobond™ 46 DLC, CrN + a-C:H:W, coating is based on the excellent load bearing and high temperature properties of Tribobond™ 30 (CrN), with an extra low friction running-in coating on top. This results in a coating system that combines excellent running-in properties, a high load carrying capacity and fatigue resistance with a good wear resistance and a low coefficient of friction.

Performance

Hard and wear resistance coatings like Tribobond™ 46 DLC offer high load bearing capabilities combined with excellent counterparts protection in order to extend the lifetime of the components.

Technical data

 

Material

Cr + CrN + a-C:H:W

Coating thickness

1 - 8 μm

Service Temp.

350 °C

Deposition Temp.

200 - 250 °C

Hardness HV 0.05

1000 – 1800 (for the a-C:H:W top layer)

Abrasive wear resistance

2 – 7 * 10-15 m³/Nm

Deposition method

PVD UBM

Friction vs. steel, dry

0.1

Color

grey